Transcript of Radiographic Interpreter: Weld Defect Exercise Part 2
ASNT RT LEVEL 2
IN-HOUSE TRAINING
AL-USWAH INSPEKSITAMA
NDT TRAINING CENTER
Jl. Raya Natar No. 55, Pasar Lama Natar Lampung Selatan
Telp. 0721-91025 / 081369255454 E-mail: [email protected]
X1
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X2
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X3
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X4
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X5
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X6
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X7
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X8
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X9
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X10
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
JAWABAN
� X1 Gas Pores
� X2 Spatter
� X3 Isolated Slag Inclusion
� X4 Elongated Cavity
� X5 Intermittent Undercut
� X6 Worm Hole
� X7 Side Wall Fusion
� X8 Distributed Porosity
� X9 Linear Slag Inclusion
� X10 Root Concavity
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER