Osprey 8+ · 2018-01-18 · Standard Osprey Distortion plus Anisotropy image side by side »...

2
STATE-OF-THE-ART DISTORTION AND ANISOTROPY MEASUREMENT ACTIONABLE DATA FOR EVERY GLASS SHEET PROCESS CONTROL TO ADDRESS TEMPERING STRESS DETECTS IRIDESCENCE DURING PRODUCTION IMPROVES QUALITY AND THROUGHPUT Osprey ® 8+ Distortion + Flatness Inspection System Developed in partnership with Stress Photonics, the global leader in optical stress analysis, and designed for installation on any brand of tempering line. Anisotropy — oſten seen as reflected iridescence — is a problem of growing interest to architects, developers, and building owners. It is a natural result of the tempering process when unbalanced residual temper stress selectively reflects polarized light. LiteSentry, with Stress Photonics offers Anisotropy Inspection integrated with the Osprey Distortion + Flatness Inspection system. With two state-of-the-art inspection systems housed in a single unit, the Osprey 8+ provides 100% inspection, offering visualization and quantification of the most challenging problems in glass fabrication. OSPREY ® 8+ Distortion + Flatness Inspection System With Anisotropy Inspection Setting the Standard in Glass Inspection With Anisotropy Inspection P S tress hotonics S tress hotonics

Transcript of Osprey 8+ · 2018-01-18 · Standard Osprey Distortion plus Anisotropy image side by side »...

Page 1: Osprey 8+ · 2018-01-18 · Standard Osprey Distortion plus Anisotropy image side by side » Osprey® 8+ with Anisotropy Inspection uses Stress Photonics Grey-Field Polariscope cameras

S TAT E - O F -T H E - A R T

D I S T O R T I O N A N D

A N I S O T R O P Y

M E A S U R E M E N T

A C T I O N A B L E

D ATA F O R E V E R Y

G L A S S S H E E T

P R O C E S S C O N T R O L

T O A D D R E S S

T E M P E R I N G

S T R E S S

D E T E C T S

I R I D E S C E N C E

D U R I N G

P R O D U C T I O N

I M P R O V E S Q U A L I T Y

A N D T H R O U G H P U T

Osprey

® 8+Distortion + Flatness Inspection System

Developed in partnership with Stress Photonics, the global leader in optical stress analysis, and designed for installation on any brand of tempering line.

Anisotropy — often seen as reflected iridescence — is a problem of growing interest to architects, developers, and building owners. It is a natural result of the tempering process when unbalanced residual temper stress selectively reflects polarized light.

LiteSentry, with Stress Photonics offers Anisotropy Inspection integrated with the Osprey Distortion + Flatness Inspection system. With two state-of-the-art inspection systems housed in a single unit, the Osprey 8+ provides 100% inspection, offering visualization and quantification of the most challenging problems in glass fabrication.

OSPREY® 8+ Distortion + Flatness Inspection SystemWith Anisotropy Inspection

Setting the Standard in Glass Inspection

With Anisotropy Inspection

PPStress hotonicsStress hotonics

Page 2: Osprey 8+ · 2018-01-18 · Standard Osprey Distortion plus Anisotropy image side by side » Osprey® 8+ with Anisotropy Inspection uses Stress Photonics Grey-Field Polariscope cameras

Standard Osprey Distortion plus Anisotropy image side by side »

Osprey® 8+ with Anisotropy Inspection uses Stress Photonics Grey-Field Polariscope cameras and polarized transmitted light to detect anisotropy effects in every sheet of glass. Combined with its industry-leading distortion inspection capability, the Osprey offers the most complete glass inspection system for tempered glass.

» Distortion Inspection: High-resolution visible light cameras and a patented reflected white LED light source measure flatness and distortion.

» Anisotropy Inspection: Patented Grey-Field Polariscope (GFP) cameras and a patent-pending polarized transmitted light array mounted under the glass measure iridescence and average stress.

Iridescence is frequently visible when glass reflects the polarized light of blue skies or water. In these situations, light that would naturally pass through the glass rotates, causing shimmering patterns where glass stress is high and reflected, and dark patterns where stress is low and transmitted.

CONTACT US TODAY:

Jakub KowalczykSales and Marketing Manager

LiteSentrytm Corporation1403 F Heritage DriveNorthfield, Minnesota 55057 USAtel : +1.507.645.2600email : [email protected]

LiteSentry.com

» OSPREY 8 » Distortion + Flatness Inspection

» OSPREY 8+ » Distortion + Flatness with Anisotropy Inspection

» HAWK » Scratch + Defect Inspection

» OWL » Recipe Selection + Tempering Furnace Control

» RAVEN » Thickness + Coating Sensor

» FALCON » Precision Size + Geometry Inspection

» LOAD VALIDATOR » Load Geometry + Fault Condition Detection

Osprey® 8+ with Anisotropy Inspection

Osprey® 8+ with Anisotropy Inspection can be installed on any brand of tempering line:

» Fully integrated grey-field polariscope system manufactured by Stress Photonics, a leader in the optical stress analysis for over 20 years.

» Real-time inspection and data collection at four polarization states.

» A map of the predicted iridescence for every part on a scale of 0-100% of maximum possible value.

» A map of average stress for every part.

» User-defined quality thresholds for the judgment of iridescence, similar to the Osprey’s proven quality thresholding methods for optical distortion.

» Data and images of every part are saved. Traceable and audible, allowing for full accountability.

Anisotropy Iridescence results with dynamic analysis charts »