LEP and LHC double walled tubes experiences

16
LEP and LHC double walled tubes experiences Sergio Calatroni

description

LEP and LHC double walled tubes experiences. Sergio Calatroni. LEP couplers. Double walled tube – coupler extension – “chemise”. LEP Coupler “crisis” – circa 1994. Many people took part to the coupler study at that time Problem: deconditioning - PowerPoint PPT Presentation

Transcript of LEP and LHC double walled tubes experiences

LEP and LHCdouble walled tubes experiences

Sergio Calatroni

LEP couplers

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 2

Double walled tube – coupler extension – “chemise”

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 3

LEP Coupler “crisis” – circa 1994

• Many people took part to the coupler study at that time

• Problem: deconditioning– Traced back to desorption and re-adsorption of gases onto cold surfaces

• Outgassing + multipacting: solutions– Ti coating of all parts– Fixed coupler– Change impedance from 50 Ohm to 75 Ohm– Smooth surfaces with less outgassing– Bake the ceramic– DC bias– Clean room procedures

• Factual review by R. Losito CERN-SL-2002-057 ECTReview of SPL RF couplers Sergio Calatroni - 16.3.2010 4

Double walled tubes: fabrication

• 316 LN stainless steel, forged blanks• Integral machining by turning• Advantages:

– Lower Electron Stimulated Desorption– Smoothness – surface quality– Manufacturing cost in a series comparable to standard

metalworking (F. Bertinelli)

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 5

Copper coating

• Copper sputter coating preferred over electroplating• Advantages:

– Lower outgassing– Lower Electron Stimulated Desorption (ESD)– Better Thermal Desorption Spectrometry (TDS)– Satisfactory RRR

• Problem:– Difficult adhesion of copper on stainless steel

• (C. Benvenuti et al. CERN LEP2 Note 94-21)

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 6

ESD measurements (500 eV e- after 200°C / 24h bakeout)

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 7

Rolled+welded and Cu sputter coated

Full machining and Cu sputter coated

Copper ESD measurements

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 8

Cu sputter coated

Cu electroplated

Copper TDS measurements

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 9

Cu sputter coated Cu electroplated

RRR measurements

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 10

Thickness at 700 MHz: effect of RRR

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 11

RRR 10 RRR 1

Copper thickness: room temperature, 700 MHz

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 12

Ideal thickness = 4 m

Copper coating by sputtering

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 13

Adhesion of Cu on s.steel is poor because it does not bind to CrO

Idea: Ti underlayer, followed by Cu coating without breaking the vacuum. Metal-metal adhesion generally very good

Problem: BN

• Stainless steel is vacuum fired at 950 °C– 316 LN steel contains some boron to increase hot workability (a few

ppm)– If B > 9 ppm (MnS precipitates could act as possible nucleation sites) it

may segregate at the surface as BN, with thickness of several nm (S. Sgobba, EST/SM/MB 00-11-25)

– BN is hexagonal, called sometimes “white graphite”, hydrophobic– Cannot be removed by detergents– Film can peel-off

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 14

S. SgobbaM. Taborelli

Solution: BN

– Vacuum fire at 950 °C– Electropolish the surface (removes BN and becomes mirror

like)– Second vacuum firing at 950 °C to remove H2 introduced by

electropolishing– Careful to use slow temperature ramp to avoid deformation

of double wall

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 15

LHC couplers

• 260 (?) new LEP double wall tubes, very successful operation

• LHC were made following LEP recipes• Total: 25 pieces (?)

Review of SPL RF couplers Sergio Calatroni - 16.3.2010 16