The Problem:

• A Centaur with several years worth of antifouling

• Which had built up and started to crack and flake off on to the paint roller as we applied new layers.

• Under the antifouling – VC Tar Epoxy • I wanted to remove the antifouling without

losing the VC Tar.

Page 3: Epoxy Treatment of Centaur Hull

If you Do it Yourself:

• You keep at it till you get it right• You don’t worry how long that takes because

you aren’t charging yourself out at £50 per hour.

• You know it has been done properly• You learn about your boat• And you can save money.

Page 4: Epoxy Treatment of Centaur Hull

Approaches to Antifouling Removal

Slurry Blasting

Chemical Antifoul Strippers take several applications andRemoving a thick layer would be a slow business.

A good bit of kit but not easy to use on a hull with concave curves as the edges of the blade dig in.

Slurry blasting removed the VC Tar sadly, butLeft a keyed surface ideal for epoxying. NB Choose an experienced operator.

Page 5: Epoxy Treatment of Centaur Hull

Stripped Hull

• VC Tar Couldn’t be saved• Keel Epoxied immediately• We found white blobs all

over hull• Osmosis? We asked a

Surveyor who told us hull was dry and white marks were repairs to voids when hull was removed from the mould.

Page 6: Epoxy Treatment of Centaur Hull

Sanded Hull

Page 7: Epoxy Treatment of Centaur Hull

Filled Hull

All the voids and any surface damage filled using West epoxy with high density filler.

Page 8: Epoxy Treatment of Centaur Hull

Choice of Epoxy

• West or SP Epoxy

• Blakes

• International

West and SP, each coat should ideally go on to previous before completely dry - at thumbnail stage. If it dries it has to be sanded down to give a key. I didn’t have time to wait for long settled period of dry weather so not an option.

Blakes only requires 2 coats so much easier, but each coat is v thick and I wasn’t sure I could achieve uniform thickness.

International seems to be easiest to apply – goes on like paint. Comes in two colours to ensure good coverage, and 6 months can elapse between layers without needing to sand down. I went for International.

Page 9: Epoxy Treatment of Centaur Hull

The Tent

You need a tent to keep it all dry and clean. I used roofing battens wedged under the rubbing strake. Tarpaulin draped over, with gap at each end to allow airflow. The ground under the tent was covered in another old tarpaulin to prevent ground moisture coming into the tent.

Page 10: Epoxy Treatment of Centaur Hull

Epoxy Coat 6

Here you can see inside the tent. All nice and clean. I had a thermometer with humidity gauge – v. useful. One cockpit drain leaked a bit so I piped it off with a bit of hose. This is coat 6, and theoretically the last coat, but the calculations provided by International to calculate required quantity are v generous so we had plenty left over

Page 11: Epoxy Treatment of Centaur Hull

Coat 8So we did 8 coats – thought that was better than leaving it in the shed to go off. Advice: buy all in one go and get discount. Buy big tins and small tins and use the big tins first – and take the small ones back if you don’t use them.

A lovely smooth finish. We did a bit of filling after 1st coat.

We used new rollers and trays for each layer. Mixing pots – don’t re-use – you get flakes. We used plastic beer glasses, marked up in advance to get the ratio right. Replace the masking tape after 3 or 4 coats – if you don’t you might not be able to remove it. After 4 layers it was a struggle to get it off.

You have plenty of time between coats but there is a strict time limit between last epoxy and 1st antifoul. So time it to allow time for both coats.

Page 12: Epoxy Treatment of Centaur Hull

Finished!

Page 13: Epoxy Treatment of Centaur Hull

Costs and Timescale

Slurry Blast £400Surveyor £200Epoxy £350Consumables £50

Total £1000

Slurry Blast in FebruaryHull sanded off by end of

MarchVoids filled in early AprilEpoxying finished by end

April

Page 14: Epoxy Treatment of Centaur Hull

Conclusion

• Not a difficult job• Be prepared for surprises• Preparation is really important.• Get someone to help – much easier to do two

boats in company than one boat on your own.• Your boat will sail faster with a smooth

bottom.• Don’t epoxy over a wet hull.