General characteristics CSA Concrete Repair Material is a high performance blend of rapid set hydraulic cement
and quality aggregates. When mixed with water CSA Concrete Material produces a
workable, high quality concrete material that is ideal where fast strength gain, high
durability and low shrinkage are desired. CSA concrete repair material is non-metallic and
no chlorides added.
Properties 1. Dry-shrinkage ratio is less than 0.04%.
Portland cement concrete has long hardening time, and so dry shrinkage is very low. If the
shrinkage rate of repair material is too high, the original concrete and the CSA repair
concrete may have different load-bearing capacity which cause hollowing or split-off.
After decades of delving, finally we find the most suitable mix proportion to get a talent
concrete repair material which can develop a micro expansion and low shrinkage. These
properties can make the repair material combined with the original concrete surface
strongly; most of concrete repair materials in market currently can not reach.
2. Bond Strength ≥1.5Mpa.
Only the original concrete and repair material have solid combination, the concrete repair
can achieve the perfect effect. This requires repair materials have higher tensile bond
strength. The addition of polymers certainly ensures this purpose, meanwhile improving
the flexibility of the repair material.
3. Avoid cracking, falling off and breaking.
4. Freeze resistance, impermeability, good corrosion resistance.
Scientific ternary system let our repair material have a micro expansion, low water ratio,
the addition of polymer improve the density of the repair material and antifreeze,
impermeability and corrosion resistance properties.
5. Polymers and the addition of quartz sand used as aggregate material greatly
improves the wear resistance of repair materials.
6. High early strength.
Its compressive strength can reach 3.5Mpa within 6h, 35~50Mpa after 28days.
7. Easy to use.
The maximum diameter of aggregate in repair material is below 1.5mm; fully apply to all
kinds of thin patch. According to the patching thickness, 1.5~25mm size aggregate can be
added as well to increase the strength of repair material.
8. High performance and competitive price.
CSA Concrete Urgent Repair Material
Application area
Repair the surface dusting, bubbles, holes, voids and pits of the concrete.
Repair the concrete cracks.
Surface repair after grouting.
Repair and Reinforcement to concrete structure.
Urgent concrete repair works.
Bolt hole placement and equipment base second pouring.
Repair and construction of pavements
Formed work
Setting posts.
Application method
Using of CSA Concrete Repair Material
Surface Preparation:
Where bonding is important, the adjacent surfaces shall be clean, sound and free from
any materials that may inhibit bond such as oil, asphalt, curing compounds, acids, dirt and
loose debris. Roughen surfaces and remove all unsound concrete. Moisten the surface
well but keep no residue water left when repair works begin. Don’t coat any interface
agent on the base surface.
Mixing:
The use of a power driven mechanical mixer, such as a mortar mixer or a drill mounted
mixer, is recommended. Organize work so that all personnel and equipment are in place
before mixing. Use clean Potable water. This material should be strictly mixed according
to instruction of specified mixed water/material ratio with blender, no hand mixing, and the
mixed slurry should be used in 40 minutes.
Placement:
CSA Concrete Repair Material may be placed using traditional methods. Organize work
so that all personnel and equipment are ready before placement. Place, consolidate and
screed quickly to allow for maximum finishing time. Do NOT wait for bleed water, apply
final finish as soon as possible. CSA Concrete Repair Material may be troweled, floated or
broom finished. On flat work, install CSA Concrete repair material in layers,DO NOT install
full depth sections and progress horizontally. Do NOT install on frozen surfaces. Use a
method of consolidation that eliminates air voids. To extend working time, retarding
admixture can be applied.
Temperature:
Warm environmental and materials temperatures will reduce the working time of CSA
Concrete Repair Material Mix. To compensate for warm temperatures, keep material cool
and use chilled mix water. Temperatures below 20ºC will decrease the rate of strength
gain and CSA Concrete Repair Material Mix should not be applied if surface or ambient
temperature is below 5ºC.
Storgae
Package and Storage
1. Packed in a 25kg plastic and paper compound bag.
2. The product should be stored in dry place. Shelf life is 3 months.
Note: Edit by Jack Young, 2014-05-12,as references only. For more informations, please
contact: cell phone no.: +0086 158 1032 6158 or mail box: [email protected]
online: [email protected] (MSN) yangjian1886 (Skype)