10/27/14

Keysight G200 Nanoindenter (formerly Agilent)

Location White Bldg. Room 613

10/27/14 Keysight Nanoindenter (formerly Agilent)

10/27/14 Keysight Nanoindenter

Capabilities: • Determining Modulus at specified depth. •Using Continuous Stiffness Module to determine Modulus as a function of depth (CSM). •Determining modulus and hardness though the thickness of coatings.

10/27/14 Keysight Nanoindenter

Sample Tray

(4) Samples can be loaded at one time.

Sample size limitation 30 mm diameter x 25-28 mm tall cylinder

10/27/14 Keysight Nanoindenter

Quick access to samples without exchange of entire environment.

10/27/14 Keysight Nanoindenter

Data / Results are displayed and exported easily to Excel.

-50

0

50

100

150

200

250

300

-200 0 200 400 600 800 1000 1200 1400 1600

mN

nm

Loading / Unloading on Calibration Standard – Fused Silica

10/27/14 Nanoindenter Example Output

10/27/14

More information can be located @ Keysight’s website:

10/27/14